SAE AMS5834C Cobalt Alloy, Corrosion and Heat-Resistant, Round Wire 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Vacuum Induction Plus Consumable Electrode Melted Solution Heat Treated, Cold Drawn, and Aged standard by SAE International, 10/02/2003
SAE AMS5833C Cobalt Alloy, Corrosion and Heat-Resistant, Round Wire 20Cr - 15Ni - 40Co - 7.0Mo - 16Fe Solution Heat Treated and Cold Drawn standard by SAE International, 10/02/2003
SAE AMS5749E Steel, Corrosion-Resistant, Bars, Wire, Forgings, and Tubing 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C) Premium Quality for Bearing Applications, Double Vacuum Melted standard by SAE International, 10/02/2003
SAE AMS4437E Magnesium Alloy Castings, Sand 8.7Al - 0.70Zn (AZ91C-T6) Solution Heat Treated and Aged standard by SAE International, 10/02/2003
SAE AMS7855C Columbium (Niobium) Alloy Bars, Rods, and Wire 10W 2.5Zr Recrystallized ( Reaffirmed: Jun 2008 ) standard by SAE International, 10/01/2003
SAE AMS7852B Columbium (Niobium) Alloy Sheet, Strip, and Plate, 10Hf 1.0Ti ( Reaffirmed: Jun 2008 ) standard by SAE International, 10/01/2003
SAE AMS7851C Columbium (Niobium) Alloy Foil, Sheet, Strip and Plate, 10W 2.5Zr Recrystallized ( Reaffirmed: Jun 2008 ) standard by SAE International, 10/01/2003
SAE J2638_200310 Fifth Wheel and Gooseneck Attachment Performance Up to 13 608/kg (30 000/lb) Trailer GVW standard by SAE International, 10/01/2003
SAE AMS6468D Steel, Welding Wire 1.0Cr 10Ni 3.8Co 0.45Mo 0.08V (0.14-0.17C) Vacuum Melted, Environment Controlled Packaging ( Reaffirmed: Apr 2008 ) standard by SAE International, 10/01/2003
SAE AMS7857B Columbium (Niobium) Alloy Bars, Rods, and Extrusions 10Hf 1.0Ti Recrystallization Annealed ( Reaffirmed: Jun 2008 ) standard by SAE International, 10/01/2003
SAE AMS6371J Steel, Mechanical Tubing 0.95Cr 0.20Mo (0.28-0.33C) (SAE 4130) ( Reaffirmed: Apr 2008 ) standard by SAE International, 10/01/2003
SAE AMS6349C Steel Bars 0.95Cr 0.20Mo (0.38-0.43C) (SAE 4140) Normalized ( Reaffirmed: Apr 2008 ) standard by SAE International, 10/01/2003